this post was submitted on 06 Nov 2023
33 points (94.6% liked)

3DPrinting

15276 readers
139 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Hey everyone.

I built an mk3s+ from its kit form successfully, tested a few PLA prints with the stock 0.4 nozzle.

I've set prusaslicer to use a 0.6 nozzle now that I've upgraded, and am using PETG. Prints look pretty bad, in spite of calibrating z-offset etc.

If you were doing something like this for the first time, what would your setup steps be like?

To be specific, using a diamondback 0.6 nozzle, matterhackers PETG at 235c.

Issues I'm seeing are a really bad loss of detail, lots of stringing, etc.

eta: added a photo of a moderately post-processed part. Notice how rough the top surface looks, there's a disconnect between perimeter loops, etc.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 1 points 10 months ago (1 children)

Z was recalibrated already. I'll try a 50c bake for a few hours to get rid of moisture.

Ordinarily, I'd expect to see evidence of bubbling/snapping at the nozzle as water boils out while laying down plastic. No obvious signs of that though.

[–] [email protected] 2 points 10 months ago* (last edited 10 months ago)

Stringing and nozzle buildup are the general signs I get with petg being damp, extreme cases it'll have noticeable bubble, I've found that I need to run 12+ hours at 54c to dry it sufficiently, even on relatively fresh spools depending on the supplier, age etc. I also recommend securing your spools if they're paper based, had the adhesive melt on one and the entire thing fall to pieces, I just rewound it onto an empty plastic spool I had.